Deposition of NiAl/Al 3 Ni 2 (CrB 2 ) Coatings from Ni, Al and CrB 2 Powders Using Mechanical Synthesis in Planetary Ball Mill.

Maciej SzlezyngerDaniel TobołaJerzy Morgiel
Published in: Materials (Basel, Switzerland) (2024)
Interest in composite thick coatings with an intermetallic matrix stimulates the development of new deposition techniques like the co-milling of pre-alloyed NiAl powder with platelet-shaped substrates. Obtained coatings were up to several micrometers thick as cold-welding of intermetallic particles was effective only at the start of this process, while later, chipping prevailed over added material. The present experiment covered the co-milling in the planetary ball mill of Ni and Al elemental powders (1:1 molar ratio) with AISI 304 steel platelets for 32 h at 300 rpm. Next, this process was repeated with an admixture of 15 wt.% of CrB 2 powder. In both cases, their milling succeeded in producing up to a 200 μm coating after 4 h. The use of light, scanning and transmission electron microscopy (LM/SEM/TEM) helped to establish that the coatings had gradient microstructures with more refined crystallites of NiAl, Al 3 Ni 2 and CrB 2 closer to the surface. With the addition of a ceramic phase, the coatings presented higher hardness and lower friction during dry wear tests both at RT and at 500 °C.
Keyphrases
  • electron microscopy
  • metal organic framework
  • transition metal
  • high resolution
  • mass spectrometry