Impact of Different Mineral Reinforcements on HDPE Composites: Effects of Melt Flow Index and Particle Size on Physical and Mechanical Properties.
Pedro Henrique Poubel Mendonça da SilveiraMarceli do Nascimento da ConceiçãoDavi Nascimento de PinaPedro Afonso de Moraes PaesAndré Ben-Hur da Silva FigueiredoNeyda de La Caridad Om TapanesRoberto Carlos C RibeiroDaniele Cruz BastosPublished in: Polymers (2024)
The use of mineral reinforcements in polymer matrix composites has emerged as an alternative for sustainable production, reducing waste and enhancing the physical and mechanical properties of these materials. This study investigated the impact of the melt flow index (MFI) of HDPE and the particle size of two mineral reinforcements, Bahia Beige (BB) and Rio Grande do Norte Limestone (CRN), on the composites. All composites were processed via extrusion, followed by injection, with the addition of 30 wt.% reinforcement. Chemical analyses revealed similar compositions with high CaO content for both minerals, while X-ray diffraction (XRD) identified predominantly calcite, dolomite, and quartz phases. Variations in the MFI, reinforcement type, and particle size showed a minimal influence on composite properties, supported by robust statistical analyses that found no significant differences between groups. Morphological analysis indicated that composites with lower MFI exhibited less porous structures, whereas larger particles of BB and CRN formed clusters, affecting impact resistance, which was attributed to poor interfacial adhesion.
Keyphrases
- reduced graphene oxide
- physical activity
- mental health
- aqueous solution
- high resolution
- visible light
- gold nanoparticles
- magnetic resonance
- heavy metals
- magnetic resonance imaging
- ultrasound guided
- computed tomography
- risk assessment
- atomic force microscopy
- crystal structure
- single molecule
- contrast enhanced
- data analysis