Flexural strength, surface roughness, and biofilm formation of ceramic-reinforced PEEK: An in vitro comparative study.

Lolowh AlmogbelRamtin Sadid ZadehAhmet OrgevGülce ÇakmakRui Li
Published in: Journal of prosthodontics : official journal of the American College of Prosthodontists (2023)
The flexural strength of tested materials was within acceptable limits for clinical use as a denture base material. Ceramic-reinforced PEEK had the highest surface roughness; however, its similarity in biofilm formation to other groups indicates its clinical acceptability as denture base material. This article is protected by copyright. All rights reserved.