In vitro biodegradation behavior of biodegradable hydroxyapatite coated AZ31 alloy treated at various pH values.

Le HanhLe Van HaiNguyen The HoangDo Thi Hong HanhLe Minh HaiNguyen Viet Nam
Published in: Journal of applied biomaterials & functional materials (2021)
AZ31 alloy coated with HA at pH 7.5 has lowest biodegradation rate and become suitable for applications in biodegradable implants.