Effect of Polywave and Monowave Light Curing Units on the Microtensile Bond Strength and Failure Types of Different Bulk-Fill Resin Composites: An in vitro Study.

Leonor Castro-RamirezMaría Espinoza-SalcedoJosé Huamani-EchaccayaMarysela Ladera-CastañedaLuis Cervantes-GanozaEmily Hernández-HuamaníRosa Aroste-AndíaPercy Gavilán-ChávezCésar Félix Cayo-Rojas
Published in: Clinical, cosmetic and investigational dentistry (2024)
The presence of alternative photoinitiator systems that are more reactive than camphorquinone produced higher microtensile bond strength in Tetric N-Ceram Bulk Fill and Opus Bulk Fill resins when light-cured with a high and standard polywave unit, respectively, compared to Filtek One Bulk Fill resins. Finally, Tetric N-Ceram Bulk Fill and Opus Bulk Fill resins had the highest percentage of mixed failures, while Filtek One Bulk Fill resin had adhesive failures, which was related to its lower microtensile bond strength.