Inducing nematic ordering of cellulose nanofibers using osmotic dehydration.

Valentina GucciniShun YuMichael AgtheKorneliya GordeyevaYulia TrushkinaAndreas FallChristina SchützGermán Salazar-Alvarez
Published in: Nanoscale (2018)
The formation of nematically-ordered cellulose nanofiber (CNF) suspensions with an order parameter fmax≈ 0.8 is studied by polarized optical microscopy, small-angle X-ray scattering (SAXS), and rheological measurements as a function of CNF concentration. The wide range of CNF concentrations, from 0.5 wt% to 4.9 wt%, is obtained using osmotic dehydration. The rheological measurements show a strong entangled network over all the concentration range whereas SAXS measurements indicate that at concentrations >1.05 wt% the CNF suspension crosses an isotropic-anisotropic transition that is accompanied by a dramatic increase of the optical birefringence. The resulting nanostructures are modelled as mass fractal structures that converge into co-existing nematically-ordered regions and network-like regions where the correlation distances decrease with concentration. The use of rapid, upscalable osmotic dehydration is an effective method to increase the concentration of CNF suspensions while partly circumventing the gel/glass formation. The facile formation of highly ordered fibers can result in materials with interesting macroscopic properties.
Keyphrases
  • high resolution
  • high speed
  • ionic liquid
  • single molecule
  • mass spectrometry
  • high throughput
  • silver nanoparticles
  • quantum dots
  • aqueous solution
  • gold nanoparticles
  • wound healing
  • single cell
  • hyaluronic acid