Nickel deposition and penetration into the stratum corneum after short metallic nickel contact: An experimental study.
Malin Glindvad AhlströmKlara MidanderTorkil MennéCarola LidénJeanne D JohansenAnneli JulanderJacob Pontoppidan ThyssenPublished in: Contact dermatitis (2018)
Nickel deposition and SC penetration is considerable after nickel skin exposure of 3 × 10 minutes. Combined with the allergic responses resulting from the same exposures reported previously, this study highlights that short skin exposure to nickel-releasing items may cause allergic nickel dermatitis.