Modification of the contact surfaces for improving the puncture resistance of laminar structures.

Pengfei WangJinglei YangXin LiMao LiuXin ZhangDawei SunChenlu BaoGuangfa GaoMohd Yazid YahyaSonglin Xu
Published in: Scientific reports (2017)
Uncovering energy absorption and surface effects of various penetrating velocities on laminar structures is essential for designing protective structures. In this study, both quasi-static and dynamic penetration tests were systematical conducted on the front surfaces of metal sheets coated with a graphene oxide (GO) solution and other media. The addition of a GO fluid film to the front impact surface aided in increasing the penetration strength, improving the failure extension and dissipating additional energy under a wide-range of indentation velocity, from 3.33 × 10-5 m/s to 4.42 m/s. The coated -surfaces improved the specific energy dissipation by approximately 15~40% relative to the dry-contact configuration for both single-layer and double-layer configurations, and specific energy dissipations of double-layer configurations were 20~30% higher than those of the single-layer configurations. This treatment provides a facile strategy in changing the contact state for improving the failure load and dissipate additional energy.
Keyphrases
  • high resolution
  • biofilm formation
  • reduced graphene oxide
  • ultrasound guided
  • quantum dots
  • gold nanoparticles