HF etching of CAD/CAM materials: influence of HF concentration and etching time on shear bond strength.

Antonio StrafaceLena RuppAiste GintauteJens FischerNicola U ZitzmannNadja Rohr
Published in: Head & face medicine (2019)
Within the limitations of this study the recommended surface pretreatment of silicate ceramics is HF etching with concentrations of 5% or 9% for 15 s to 60s to achieve highest shear bond strength while the glassy matrix is sufficiently dissolved. The tested resin composite cements can be applied with all tested materials and suggested for clinical application.