Metal-ceramic bond strength between a feldspathic porcelain and a Co-Cr alloy fabricated with Direct Metal Laser Sintering technique.

Konstantinos DimitriadisKonstantinos SpyropoulosTriantafillos Papadopoulos
Published in: The journal of advanced prosthodontics (2018)
Specimens produced by the DMLS technique cover the lowest acceptable metal-ceramic bond strength of 25 MPa specified in ISO 9693 and present satisfactory bond strength for clinical use.