The Assessability of Approximal Secondary Caries of Non-Invasive 3D-Printed Veneers Depending on the Restoration Thickness-An In Vitro Study.
Elisabeth PrauseJeremias HeyFranziska SchmidtRobert NicicFlorian BeuerAlexey UnkovskiyPublished in: Bioengineering (Basel, Switzerland) (2023)
To date, no scientific data is available regarding the development and radiographic assessment of approximal caries development after the insertion of 3D-printed, non-invasive veneers of different restoration thicknesses. For the present study, non-invasive veneers were fabricated from two different materials for printing and milling (Vita Enamic and VarseoSmile Crown plus). Three different restoration thicknesses (0.5, 0.7, and 0.9 mm) were selected. After digital design, leaving the approximal space free, and manufacturing of the restorations, adhesive insertion followed. All specimens were placed in a demineralizing solution for 28 days. Subsequently, a radiological and fluorescent examination was performed. The present study showed statistically significant interactions for the day ( p < 0.0001) and manufacturing method ( p < 0.0001) but not for restoration thickness. Additive manufactured restorations showed less radiological caries progression compared to subtractive manufactured restorations after 21 and 28 days (0.7 and 0.9 mm restoration thickness) ( p < 0.0001). DIAGNOdent proved that the restoration thickness affected the caries progression within the subtractive group ( p < 0.0001). Radiographic and fluorescence examination showed equivalent results regarding approximal caries assessment. For additive manufacturing, less caries progression was shown without consideration of the restoration thickness.