Comparative In Vitro Study of the Bond Strength of Composite to Carbon Fiber Versus Ceramic to Cobalt-Chromium Alloys Frameworks for Fixed Dental Prostheses.
Rocio Cascos-SanchezPedro Molinero-MourelleRocio OrtegaRuben Agustin-PanaderoJaime Del Rio HighsmithMiguel Gomez-PoloPublished in: Materials (Basel, Switzerland) (2020)
The chrome-cobalt/ceramic group showed greater bonding strength compared to the carbon-fiber-reinforced composite; most of the fractures within the cobalt-chrome/ceramic group, had no possibility of direct clinical repair.