Biocompatibility of mineral trioxide aggregate flow and biodentine.

J A S MondelliR A HoshinoP H WeckwerthPaulo Sergio CerriR T LeonardoJ M Guerreiro-TanomaruMario Tanomaru-FilhoGuilherme Ferreira da Silva
Published in: International endodontic journal (2018)
Although thick MTA Flow induced a less intense inflammatory response, all evaluated materials are biocompatible because they allowed regression of this process after 60 days.