Login / Signup

Dissolution of Platinum Single Crystals in Acidic Medium.

Daniel John Seale SandbeckOlaf BrummelKarl J J MayrhoferJoerg LibudaIoannis KatsounarosSerhiy Cherevko
Published in: Chemphyschem : a European journal of chemical physics and physical chemistry (2019)
Platinum single crystal basal planes consisting of Pt(111), Pt(100), Pt(110) and reference polycrystalline platinum Pt(poly) were subjected to various potentiodynamic and potentiostatic electrochemical treatments in 0.1 M HClO4 . Using the scanning flow cell coupled to an inductively coupled plasma mass spectrometer (SFC-ICP-MS) the transient dissolution was detected on-line. Clear trends in dissolution onset potentials and quantities emerged which can be related to the differences in the crystal plane surface structure energies and coordination. Pt(111) is observed to have a higher dissolution onset potential while the generalized trend in dissolution rates and quantities was found to be Pt(110)>P(100)≈Pt(poly)>Pt(111).