The Influence of Saliva pH on the Fracture Resistance of Three Complete Denture Base Acrylic Resins.
Juliana de SáFrancisca VieiraCarlos Manuel ArosoMónica CardosoJosé Manuel MendesAntonio Sergio SilvaPublished in: International journal of dentistry (2020)
It can be concluded within the limitations of this study that there are differences in the fracture resistance among the three brands of acrylic resin. Megacryl® was found to have the highest fracture resistance, and Triplex Hot® was the lowest. The results also show that exposure to a low pH environment decreases the fracture resistance of the Megacryl® and RS Vertex® resins.