A Comparison of Hydrogen Storage in Pt, Pd and Pt/Pd Alloys Loaded Disordered Mesoporous Hollow Carbon Spheres.
Martyna BacaKrzysztof CendrowskiWojciech KukułkaGrzegorz BazarkoDariusz MoszyńskiBeata MichalkiewiczRyszard J KalenczukBeata ZielinskaPublished in: Nanomaterials (Basel, Switzerland) (2018)
Comprehensive study to evaluate the ability of hydrogen uptake by disordered mesoporous hollow carbon spheres doped witch metal such as Pt, Pd or Pt/Pd was conducted. They were synthesized facilely using sonication and then calcination process under vacuum at the temperature of 550 °C. The effect on hydrogen sorption at neat-ambient conditions (40 °C, up to 45 bar) was thoroughly analyzed. The results clearly revealed that metal functionalization has a significant impact on the hydrogen storage capacity as the mechanism of gas uptake depends on two factors: metal type and certain size of particles. Thus, functionalized spheres adsorb hydrogen by physisorption forming metal hydrides or metal hydrides combined with hydrogen spillover effect. As a result, a sample with narrower distribution of nanoparticles and smaller specific size exhibited enhanced hydrogen uptake.