LaFe 0.4 Ni 0.6 O 3 /CeO 2 (1:1) two-phase composite materials were prepared by mechanochemical (MC) and Pechini routes. The catalytic properties of the composites in methane and CO oxidation reactions strongly depend on their preparation conditions. In low-temperature (<600 °C) catalytic CO oxidation the composites demonstrate a higher activity compared with LaFe 0.4 Ni 0.6 O 3 perovskite. The highest activity was observed for the composite prepared by mechanical treatment of perovskite and fluorite precursors. There is a correlation between activity and the content of weakly bound surface oxygen species. Catalytic activity in high-temperature (>750 °C) catalytic methane oxidation correlates with the reducibility of samples. The highest activity was observed for the composite prepared by the one-pot Pechini route with higher reducibility of the sample up to 600 °C.
Keyphrases
  • hydrogen peroxide
  • visible light
  • room temperature
  • high temperature
  • reduced graphene oxide
  • nitric oxide
  • high efficiency
  • aqueous solution