Tear strength and elastic recovery of new generation hybrid elastomeric impression material: A comparative study.

Lamia SingerChristoph BourauelShaymaa I HabibHeba El-Amin ShalabySayed H Saniour
Published in: BMC research notes (2022)
A polyether (PE), polyvinyl siloxanse (PVS) and vinyl polyether silicone (VPES) hybrid elastomers were used in the present study. Tear strength was measured one hour after setting time of each material according to the manufacturer and the three materials showed statistically comparable tear strength in N/mm. Elastic recovery was evaluated one minute after the setting time recommended by the manufacturer. The three materials were statistically insignificant from each other, and all met the ISO4823 requirement of having greater than 96.5% recovery.