Effect of thermal treatment on the stability of Na-Mn-W/SiO2 catalyst for the oxidative coupling of methane.

Dorota MatrasAntonios VamvakerosSimon D M JacquesNicolas GrosjeanBenjamin RollinsStephen PoulstonGavin B G StenningHamid R GodiniJakub DrnecRobert J CernikAndrew M Beale
Published in: Faraday discussions (2021)
In this study, we investigate the effect of thermal treatment/calcination on the stability and activity of a Na-Mn-W/SiO2 catalyst for the oxidative coupling of methane. The catalyst performance and characterisation measurements suggest that the W species are directly involved in the catalyst active site responsible for CH4 conversion. Under operating conditions, the active components, present in the form of a Na-W-O-Mn molten state, are highly mobile and volatile. By varying the parameters of the calcination protocol, it was shown that these molten components can be partially stabilised, resulting in a catalyst with lower activity (due to loss of surface area) but higher stability even for long duration OCM reaction experiments.
Keyphrases
  • room temperature
  • ionic liquid
  • metal organic framework
  • carbon dioxide
  • reduced graphene oxide
  • highly efficient
  • randomized controlled trial
  • gold nanoparticles
  • visible light
  • high resolution
  • genetic diversity