Login / Signup

Analyzing the Role of Fe 0 and Fe 3+ in the Formation of Expanded Clay Aggregates.

José Manuel Moreno-MarotoBeatriz González-CorrochanoAna M Martínez-RodríguezAntonio Conde-SánchezCarlos Javier Cobo-CeaceroJacinto Alonso-AzcárateManuel Uceda-RodríguezAna B LópezCarmen Martínez GarcíaMaría Teresa Cotes-Palomino
Published in: Materials (Basel, Switzerland) (2023)
The effect of the addition of Fe 0 and Fe 3+ on the formation of expanded clay aggregates was studied using iron-free kaolin as an aluminosilicates source. Likewise, the incorporation of cork powder as a source of organic carbon and Na 2 CO 3 as a flux in the mixtures was investigated in order to assess its effect in combination with the iron phases. An experimental protocol, statistically supported by a mixture experiments/design of experiments approach, was applied to model and optimize the bloating index, density, absorption capacity, and mechanical strength. The process of expansion and pore generation and the associated decrease in density required the addition of iron, such that the optimum mixtures of these properties presented between 25 and 40 wt.% of Fe 0 or Fe 3+ , as well as the incorporation of 3.5-5 wt.% of organic carbon. The addition of Fe 3+ produced a greater volumetric expansion (max. 53%) than Fe 0 (max. 8%), suggesting that the formation of the FeO leading to this phenomenon would require reducing and oxidizing conditions in the former and the latter, respectively. The experimental and model-estimated results are in good agreement, especially in the aggregates containing Fe 0 . This reinforces the application of statistical methods for future investigations.
Keyphrases
  • metal organic framework
  • aqueous solution
  • randomized controlled trial
  • visible light
  • mass spectrometry
  • current status
  • solid state